Our personnel are generally within the spirit of “continuous improvement and excellence”, and using the excellent top quality goods, favorable rate and superior after-sales expert services, we try to win every customer’s believe in for Wholesale Discount 99.95 Tzm Molybdenum Electrode Bar For Glass Melting Vacuum Furnace, To significantly improve our service quality, our company imports a large number of foreign advanced devices. Welcome clients from home and abroad to call and inquire!
Our personnel are generally within the spirit of “continuous improvement and excellence”, and using the excellent top quality goods, favorable rate and superior after-sales expert services, we try to win every customer’s believe in for Molybdenum Bar, Molybdenum Electrode Bar In Vacuum Furnace, Tzm Molybdenum Rod/bar, We expect to provide solutions and services to more users in global aftermarket markets; we launched our global branding strategy by providing our excellent merchandise all over the world by virtue of our well reputed partners letting global users keep pace with technology innovation and achievements with us.
TZM rods
Chemical composition:
Main and minor components | Min.content(%) | ASTM B386 (361) |
Mo | blance | balance |
Ti | 0.40-0.55% | 0.40-0.55% |
Zr | 0.06-0.12% | 0.06-0.12% |
Impurities | Max.values (μg/g) | Max.values (μg/g) |
Al | 10 | - |
Cu | 20 | - |
Cr | 20 | - |
Fe | 20 | 100 |
K | 20 | - |
Ni | 10 | 50 |
Si | 20 | 50 |
W | 300 | - |
C | 100-400 | 100-400 |
H | 10 | - |
N | 10 | 20 |
O | 500 | 300 |
Cd | 5 | - |
Hg | 1 | - |
Pb | 5 | - |
Dimensions and tolerances:
Diameter (mm) | Diameter tolerance (mm) |
Ground | |
0.50-0.99 | ±0.007 |
1.00-1.99 | ±0.010 |
1.00-2.99 | ±0.015 |
3.00-15.9 | ±0.020 |
16.0-24.9 | ±0.030 |
25.0-34.9 | ±0.050 |
35.0-3939 | ±0.060 |
≥40.0 | ±0.20 |
Cleaned | |
0.50-4.0 | ±2.0% |
4.10-10.0 | ±1.5% |
15.0-50.0 | ±0.30 |
51.0-75.0 | ±0.40 |
75.1-120.0 | ±1.00 |
121.0-165.0 | ±1.50 |
Turned | |
40.0-49.9 | ±0.30 |
50.0-165.0 | ±0.40 |
Length and straightness:
Diameter (mm) | Production length (mm) | Stiraightness/Meter (mm) | |
Cleaned | Ground/turned | ||
0.50-0.99 | >500 | <2.5 | <2.5 |
1.00-9.90 | >300 | <2.0 | <1.5 |
10.0-165.0 | >100 | <1.5 | <1.0 |
Length tolerance:
Diameter 0.50-30.0 mm | ||||||
Nominal length (mm) | 6-30 | 30-120 | 120-400 | 400-1000 | 1000-2000 | >2000 |
Length tolerance(mm) | ±0.2 | ±0.3 | ±0.5 | ±0.8 | ±1.2 | ±2.0 |
Diameter >30.0 mm | ||||||
Nominal length (mm) | 6-30 | 30-120 | 120-400 | 400-1000 | 1000-2000 | >2000 |
Length tolerance(mm) | ±1.0 | ±1.5 | ±2.5 | ±4.0 | ±6.0 | ±8.0 |
Density:
1. 0.50-40.0 mm ≥10.15g/cm³
2. 40.1-80.0 mm ≥10.10g/cm³
3. 80.1-120.0 mm ≥10.00g/cm³
4. 120.1-165.0 mm ≥9.90g/cm³
Nondestructive testing: For diameters>15.00 mm:100% ultrasonic testing; For diameters of 0.50-50.0mm:Eddy curent tests on rods with ground.
Diameter(mm) | Tensile strength(MPa) | 0.2% Yield Strength(MPa) | Elongation(%) | Hardness(HV 10) |
0.50-4.76 | - | - | - | - |
4.76-22.20 | ≥790 | ≥690 | ≥18 | |
22.20-28.60 | ≥760 | ≥655 | ≥15 | 260-320 |
28.60-47.60 | ≥690 | ≥585 | ≥10 | 250-310 |
47.60-73.00 | ≥620 | ≥550 | ≥10 | 245-300 |
73.00-120.9 | ≥585 | ≥515 | ≥5 | 240-290 |
121.0-165 | ≥585 | ≥515 | ≥5 | 220-280 |
Surface condition:
Surface: | Cleaned | Ground | Turned |
φ0.50-165mm | φ0.50-50.00mm | φ≥40.00mm | |
Roughness | Diameter (mm) | Ra (μm) Ground | Ra (μm) Turned |
≤2.50 | ≤0.80 | - | |
2.5-50.0 | ≤1.00 | - | |
≥40.0 | - | ≤3.2 |