Our advancement depends over the superior machines, exceptional talents and continually strengthened technology forces for Pure Tungsten Rod, Tungsten Rod, We aim to become the modern enterprise with the commercial ideal of “Sincerity and confidence” and with the aim of “Offering customers the most sincere services and best quality products”. We sincerely ask for your unchanged support and appreciate your kind advice and guidance.
TZM rods
Chemical composition:
Main and minor components | Min.content(%) | ASTM B386 (361) |
Mo | blance | balance |
Ti | 0.40-0.55% | 0.40-0.55% |
Zr | 0.06-0.12% | 0.06-0.12% |
Impurities | Max.values (μg/g) | Max.values (μg/g) |
Al | 10 | - |
Cu | 20 | - |
Cr | 20 | - |
Fe | 20 | 100 |
K | 20 | - |
Ni | 10 | 50 |
Si | 20 | 50 |
W | 300 | - |
C | 100-400 | 100-400 |
H | 10 | - |
N | 10 | 20 |
O | 500 | 300 |
Cd | 5 | - |
Hg | 1 | - |
Pb | 5 | - |
Dimensions and tolerances:
Diameter (mm) | Diameter tolerance (mm) |
Ground | |
0.50-0.99 | ±0.007 |
1.00-1.99 | ±0.010 |
1.00-2.99 | ±0.015 |
3.00-15.9 | ±0.020 |
16.0-24.9 | ±0.030 |
25.0-34.9 | ±0.050 |
35.0-3939 | ±0.060 |
≥40.0 | ±0.20 |
Cleaned | |
0.50-4.0 | ±2.0% |
4.10-10.0 | ±1.5% |
15.0-50.0 | ±0.30 |
51.0-75.0 | ±0.40 |
75.1-120.0 | ±1.00 |
121.0-165.0 | ±1.50 |
Turned | |
40.0-49.9 | ±0.30 |
50.0-165.0 | ±0.40 |
Length and straightness:
Diameter (mm) | Production length (mm) | Stiraightness/Meter (mm) | |
Cleaned | Ground/turned | ||
0.50-0.99 | >500 | <2.5 | <2.5 |
1.00-9.90 | >300 | <2.0 | <1.5 |
10.0-165.0 | >100 | <1.5 | <1.0 |
Length tolerance:
Diameter 0.50-30.0 mm | ||||||
Nominal length (mm) | 6-30 | 30-120 | 120-400 | 400-1000 | 1000-2000 | >2000 |
Length tolerance(mm) | ±0.2 | ±0.3 | ±0.5 | ±0.8 | ±1.2 | ±2.0 |
Diameter >30.0 mm | ||||||
Nominal length (mm) | 6-30 | 30-120 | 120-400 | 400-1000 | 1000-2000 | >2000 |
Length tolerance(mm) | ±1.0 | ±1.5 | ±2.5 | ±4.0 | ±6.0 | ±8.0 |
Density:
1. 0.50-40.0 mm ≥10.15g/cm³
2. 40.1-80.0 mm ≥10.10g/cm³
3. 80.1-120.0 mm ≥10.00g/cm³
4. 120.1-165.0 mm ≥9.90g/cm³
Nondestructive testing: For diameters>15.00 mm:100% ultrasonic testing; For diameters of 0.50-50.0mm:Eddy curent tests on rods with ground.
Diameter(mm) | Tensile strength(MPa) | 0.2% Yield Strength(MPa) | Elongation(%) | Hardness(HV 10) |
0.50-4.76 | - | - | - | - |
4.76-22.20 | ≥790 | ≥690 | ≥18 | |
22.20-28.60 | ≥760 | ≥655 | ≥15 | 260-320 |
28.60-47.60 | ≥690 | ≥585 | ≥10 | 250-310 |
47.60-73.00 | ≥620 | ≥550 | ≥10 | 245-300 |
73.00-120.9 | ≥585 | ≥515 | ≥5 | 240-290 |
121.0-165 | ≥585 | ≥515 | ≥5 | 220-280 |
Surface condition:
Surface: | Cleaned | Ground | Turned |
φ0.50-165mm | φ0.50-50.00mm | φ≥40.00mm | |
Roughness | Diameter (mm) | Ra (μm) Ground | Ra (μm) Turned |
≤2.50 | ≤0.80 | - | |
2.5-50.0 | ≤1.00 | - | |
≥40.0 | - | ≤3.2 |